Refilling Toner Carts (was RE: Rubber Restorer...)

From: UberTechnoid_at_home.com <(UberTechnoid_at_home.com)>
Date: Thu Nov 8 18:08:58 2001

A bead blaster would give you that satin finish in no time flat...

Regards,

Jeff

>> About the only common material that sodium hydroxide will attack is
>> aluminium, and then only when concentrated or exposure is reasonably long;
>> it has no effect on copper, steel, etc.

>Yeah, I've relied on this as a way to make satin-finish aluminum front
>panels for equipment. As the reaction progresses, the NAO2 (?) solution
>has to be preiodlically replaced. It generally took me about two days to
>get the desired look.

>-dq

-- 
-----------------------------------------------------------
Jeffrey S. Worley
Asheville, NC USA
828-6984887
UberTechnoid_at_Home.com
-----------------------------------------------------------
Received on Thu Nov 08 2001 - 18:08:58 GMT